Arkema Group Rilsan® AZM 23 T6LD Nylon 12, 23% Glass Fiber Filled (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 12 , Nylon 12, 20% Glass Fiber Filled
Manufacturer Arkema
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Arkema Group Rilsan® AZM 23 T6LD Nylon 12, 23% Glass Fiber Filled (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Designation ISO 1874-PA12,MHLR,16-050,GF23Rigid grade with glass fiber filler (23%) for injection molding. Available colors: black and natural. Reinforced light and heat stabilizing agent. Mold-release agent.Rigidity. High compressive strength. Very low shrinkage: include 0,5% on average for the design of the mold. Low coefficient of linear expansion. High dimensional stability.Example applications: Rigid mechanical parts.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Melt Flow 3.2 g/10 min

@Load 2.16 kg,
Temperature 235 °C
3.2 g/10 min

@Load 4.76 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 85.0 MPa
12300 psi
5 mm/min
Elongation at Break 6.0 %
6.0 %
5 mm/min
Tensile Modulus 5.48 GPa
795 ksi
1 mm/min
Electrical Properties Metric English Comments
Dissipation Factor 0.000357

@Frequency 1e+6 Hz
0.000357

@Frequency 1e+6 Hz
0.000522

@Frequency 100 Hz
0.000522

@Frequency 100 Hz