Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon Thermavac® 0.020" (0.508 mm) Uncured Silicone Vacuum Bagging (30400R020)

Category Polymer , Thermoset , Silicone
Manufacturer Arlon
Trade Name Thermavac®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon Thermavac® 0.020" (0.508 mm) Uncured Silicone Vacuum Bagging (30400R020).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Uncured, unsupported silicone rubber with a thickness of 0.020 in ± 0.002 (0.51 mm ± 0.051) on a Kodacel carrier (0.005 in., 0.13 mm nominal thickness); 0.003 in. (0.08 mm) polyethylene interleave. The shelf life is defined as the duration of time for which the product will meet the physical requirements outlined below. It does not guarantee the product’s usefulness in all applications. Color: Red. Weight: 688.3 g/m² ± 67.8 (20.3 oz./yd.² ± 2.0). Shelf Life: 3 months from date of manufacture at 4.4°C (40°F). Cure Time: 0.5 hours. Post Cure: 204°C (400°F), for 4 hours.Applications: Composite vacuum bagging materials.Information provided by the manufacturer, Arlon Silicone Technologies Division.
Mechanical Properties Metric English Comments
Hardness, Shore A 50 - 60
50 - 60
Tensile Strength, Ultimate 6.21 - 7.59 MPa
901 - 1100 psi
Elongation at Break 450 - 550 %
450 - 550 %
Tear Strength >= 35.1 kN/m
>= 200 pli
Compression Set 28 %
28 %
after post cure
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.6 °C
-69.9 °F
Electrical Properties Metric English Comments
Dielectric Strength >= 15.75 kV/mm
>= 400.0 kV/in
Processing Properties Metric English Comments
Processing Temperature 176.6 °C
349.9 °F
curing temp., at 0.345 MPa (50 psi)