Asahi Glass Fluon® PA1020Z 20% Glass Fiber, PTFE Filled Compound

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Glass Filled, Molded
Manufacturer Asahi Glass Company
Trade Name Fluon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Glass Fluon® PA1020Z 20% Glass Fiber, PTFE Filled Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Fluon®PTFE FC has improved creep and wear resistance. A wide range of fillers such as glass fiber, graphite, bronze, carbon fiber are available. Information provided by Asahi Glass Company, Inc.
Physical Properties Metric English Comments
Specific Gravity 2.22 g/cc
2.22 g/cc
Bulk Density 0.880 g/cc
0.0318 lb/in³
Particle Size 715 µm
715 µm
Mechanical Properties Metric English Comments
Tensile Strength at Break 22.1 MPa
3210 psi
Elongation at Break 320 %
320 %
Descriptive Properties Value Comments
PTFE Content, % 80