Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Asahi Glass Fluon® PB2510 10% Carbon Fiber, PTFE Filled Compound

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Carbon Fiber Filled
Manufacturer Asahi Glass Company
Trade Name Fluon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Glass Fluon® PB2510 10% Carbon Fiber, PTFE Filled Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Fluon®PTFE FC has improved creep and wear resistance. A wide range of fillers such as glass fiber, graphite, bronze, carbon fiber are available. Information provided by Asahi Glass Company, Inc.