Asahi Kasei Thermylene® P7-30FG-0874 30% Glass Fiber Reinforced, UV Stabilized

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 30% Glass Fiber Filler
Manufacturer Asahi Kasei
Trade Name Thermylene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Kasei Thermylene® P7-30FG-0874 30% Glass Fiber Reinforced, UV Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Asahi Thermofil
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
Melt Flow 6.0 g/10 min
6.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 96.5 MPa
14000 psi
ASTM D638
Elongation at Yield 3.0 %
3.0 %
ASTM D638
Flexural Strength 134 MPa
19500 psi
ASTM D790
Flexural Modulus 5.65 GPa
820 ksi
ASTM D790
Izod Impact, Notched 1.01 J/cm
1.90 ft-lb/in
ASTM D256
Izod Impact, Unnotched 6.41 J/cm
12.0 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 154 °C
310 °F
ASTM D648