Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Axiall 10754 Wire & Cable Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 10754 Wire & Cable Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
General purpose jacket compound. Maximum service temperature rating of 75°C. Fungus resistant.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.36 - 1.40 g/cc
1.36 - 1.40 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 72 - 78
72 - 78
delayed; ASTM D-2240
Tensile Strength, Yield 13.69 MPa
1985 psi
ASTM D-638
Elongation at Yield 350 %
350 %
ASTM D-638
100% Modulus 0.00631 GPa
0.915 ksi
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 171 °C
340 °F
Users viewing this material also viewed the following: