Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Axiall 16930 Wire & Cable Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 16930 Wire & Cable Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Non-lead stabilized tray cable jacketing compound. UL recognized component for 720 hour sunlight resistance in black only.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.36 - 1.40 g/cc
1.36 - 1.40 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 90 - 96
90 - 96
delayed; ASTM D-2240
Tensile Strength, Yield 17.9 MPa
2600 psi
ASTM D-638
Elongation at Yield 174.6 %
174.6 %
Air Aging: 168 hours @ 121°C; 50 mil die-cut from jacket; UL 1581
300 %
300 %
ASTM D-638
100% Modulus 0.0138 GPa
2.00 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -22.0 °C
-7.60 °F
ASTM D-746
Oxygen Index 30 %
30 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 193 °C
380 °F