Material Notes:
THHN-THWN circuit sizes. Best suited for 105°C; 1/64 (18 AWG and larger). Rated VW-1. CSA approved TWN75, TEW, AWM IA, FT1 constructions. UL recognized for TW, THW, THWN, THHN. Oil resistant I.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.33 - 1.37 g/cc
1.33 - 1.37 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 90 - 96
90 - 96
delayed; ASTM D-2240
Hardness, Shore D 42 - 48
42 - 48
delayed; ASTM D-2240
Tensile Strength, Yield 19.82 MPa
2875 psi
ASTM D-638
Elongation at Yield 271.9 %
271.9 %
Air Aging: 168 hours @ 136°C; 30 mil slabs; UL 1581
330 %
330 %
ASTM D-638
100% Modulus 0.0128 GPa
1.85 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -22.0 °C
-7.60 °F
ASTM D-746
Oxygen Index 28 %
28 %
ASTM D-638
Electrical Properties Metric English Comments
Volume Resistivity 1.50e+15 ohm-cm
1.50e+15 ohm-cm
50% RH; ASTM D-257
Processing Properties Metric English Comments
Melt Temperature 191 °C
375 °F