Formula: C9H12OCAS: 109-53-5Description: Isobutylvinylether is a colorless liquid with an ether-like odor. It is miscible in water.Synonyms: Isobutyl-ethene, 1-Isobutoxyethylene, Isobutyl vinyl ether, VIBE, IBVE, Propane, 1-(Ethenyloxy)-2-methyl- Vinylisobutylehter, 1-(Ethenyloxy)2-methyl-propanInformation provided by BASF
Physical Properties Metric English Comments
Density 0.769 g/cc
0.0278 lb/in³
Molecular Weight 100.2 g/mol
100.2 g/mol
Thermal Properties Metric English Comments
Melting Point -112 °C
-170 °F
Boiling Point 83.0 °C
181 °F
Flash Point -15.0 °C
5.00 °F
Descriptive Properties Value Comments
Assay >99%
Composition Isobutanol
<0.1%
Ignition Temperature 198°C