Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF Pluracol® P2010 Specialty Polyol

Category Fluid
Manufacturer BASF
Trade Name Pluracol®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF BASF Pluracol® P2010 Specialty Polyol.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Pluracol® P polyols are a series of five polypropylene glycols formed by adding propylene oxide to a propylene glycol nucleus. Pluracol P1010, P2010 and 1044 (formerly P4010) are used in the preparation of polyurethane foams, adhesives, coatings, elastomers and sealants. Pluracol P410R and P710R are used in the preparation of one and two component polyurethane coatings, adhesives and elastomers.Information provided by BASF
Physical Properties Metric English Comments
Density 0.991 g/cc

@Temperature 37.8 °C
0.0358 lb/in³

@Temperature 100 °F
1.00 g/cc

@Temperature 25.0 °C
0.0361 lb/in³

@Temperature 77.0 °F
1.02 g/cc

@Temperature 60.0 °C
0.0368 lb/in³

@Temperature 140 °F
Viscosity 68 cP

@Temperature 60.0 °C
68 cP

@Temperature 140 °F
180 cP

@Temperature 37.8 °C
180 cP

@Temperature 100 °F
250 cP

@Temperature 25.0 °C
250 cP

@Temperature 77.0 °F
Molecular Weight 2000 g/mol
2000 g/mol
Thermal Properties Metric English Comments
Specific Heat Capacity 1.16 J/g-°C
0.277 BTU/lb-°F
Thermal Conductivity 0.125 W/m-K
0.868 BTU-in/hr-ft²-°F
Chemical Properties Metric English Comments
Total Acid Number <= 0.025
<= 0.025
STI 3063/3161
Processing Properties Metric English Comments
Moisture Content <= 0.040 %
<= 0.040 %
STI 3062
Descriptive Properties Value Comments
Color <20
APHA, STI 3057
Composition Na & K
<5 ppm, STI 3038
Hydroxyl Number 53.4 - 58.6 mg KOH/g
STI 3007/3162
Unsaturation <0.036 meq/g
STI 3056
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved