BASF Ultramid® A3WG3 15% Glass Filled PA66 (Conditioned)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 20% Glass Fiber Filled
Manufacturer BASF
Trade Name Ultramid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultramid® A3WG3 15% Glass Filled PA66 (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: 15% Glass-fiber reinforced and heat aging resistant injection-molding grade for machine elements and housings of medium stiffness. For electric insulating parts, preference should be given to the grades A3Eg3 and A3hg3Information provided by BASF