BASF Ultramid® A3X2G5 BK 23185 25% Glass Filled PA66 FR (Conditioned)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer BASF
Trade Name Ultramid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultramid® A3X2G5 BK 23185 25% Glass Filled PA66 FR (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: 25% glass-fiber reinforced injection-molding grade with improved flame retardance and enhanced long-term stability. Flame retardant based on red phosphorus; outstanding mechanical and electrical properties.Information provided by BASF