Material Notes:
Bapolene 200B is a low density polyethylene for blown film applications requiring superior clarity. It complies with US FDA 21CFR177.1520.Applications: General purpose, bakery, flexible, medical and industrial packaging.Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ASTM D-4883
Melt Flow 1.7 g/10 min
1.7 g/10 min
ASTM D-1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 300 %
300 %
ASTM D-882
Film Elongation at Break, TD 500 %
500 %
ASTM D-882
Elmendorf Tear Strength MD 360 g
360 g
ASTM D-1922
Elmendorf Tear Strength TD 130 g
130 g
ASTM D-1922
Dart Drop 95.0 g/micron
2410 g/mil
ASTM D-1709
Film Tensile Strength at Break, MD 24.0 MPa
3480 psi
ASTM D-882
Film Tensile Strength at Break, TD 19.0 MPa
2760 psi
ASTM D-882
1% Secant Modulus, MD 193 MPa
28000 psi
ASTM D-882
1% Secant Modulus, TD 214 MPa
31000 psi
ASTM D-882
Optical Properties Metric English Comments
Haze 8.0 %
8.0 %
<8; ASTM D-1003
Descriptive Properties Value Comments
Process Film
Region Europe/Turkey
Bamberger Polymers Distribution
International
Bamberger Polymers Distribution
Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved