Beijing Evergrow Resources ASHRAE HEPA ULPA-K79 Glass Fiber Paper

Category Ceramic , Glass , Glass Fiber
Manufacturer Beijing Evergrow Resources
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Beijing Evergrow Resources ASHRAE HEPA ULPA-K79 Glass Fiber Paper.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Fiber made from melted glass that is drawn into a thin fiber less than a thousandth of an inch in diameter. The fiber may be spun into threads and woven into fabrics which suitable for many applications ,such as removal of micron and submicron size particulates from both liquids and gases,or used in an acoustic, electrical, or thermal insulating material.Features:Lightness, heat resisting, low thermal capacity and low thermal conductivity, soft and excellent fire-isolation.Anti-heat energy and heat stability.Anti-mildew, anti-insect, un-scattered and good stretching resistance.Excellent anti-ageing.Excellent sound absorbability, adsorption and filtering.It can be cut, sewn according to requirements and it's also easy to construct.Information provided by Beijing Evergrow Resources.
Physical Properties Metric English Comments
Thickness 320 - 380 microns
12.6 - 15.0 mil
Descriptive Properties Value Comments
Air Resistance (Pa) <= 98
Efficiency (%) >= 99.99999
Mark 0.3 Micron Air Flow Rate (L/min-ºC) 0.06
Tensile Strength at Yield (N/m) 250
CD
400
MD
Weight (g/m²) 78