Beijing Evergrow Resources BF-6 Basalt Needle Felt

Category Other Engineering Material , Composite Fibers
Manufacturer Beijing Evergrow Resources
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Beijing Evergrow Resources BF-6 Basalt Needle Felt.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Basalt fiber is a material made from extremely fine fibers of basalt. It is used as a fireproof textile in the aerospace and automotive industries and can also be used as a strengthening and repairing of engineering structure products.Advantages:High strengthIncombustibleGood thermal propertiesGood insulatorWill work at 500-800 degreesInformation provided by Beijing Evergrow Resources.
Physical Properties Metric English Comments
Filament Diameter 9.0 - 13 µm
9.0 - 13 µm
Thickness 5000 - 6000 microns
197 - 236 mil
Thermal Properties Metric English Comments
Thermal Conductivity 0.0300 - 0.316 W/m-K
0.208 - 2.19 BTU-in/hr-ft²-°F
according to the difference density
Descriptive Properties Value Comments
Flammability Test Incombustible
Length (m) 50
Weight (g/m²) 800
Width (mm) 1000
Users viewing this material also viewed the following: