Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Beijing Evergrow Resources ER-13 UHMW PE Fabric

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), UHMW PE Ultra High Molecular Weight
Manufacturer Beijing Evergrow Resources
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Beijing Evergrow Resources ER-13 UHMW PE Fabric.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
UHMWPE fabric is made of high modulus, high performance polyethylene fiber which are orthogonal laid down and thermally bonded with special bulletproof binder.Features:lightweightsoft, flexiblewaterproofoutstanding UV resistancemoisture resistanthigh energy absorptionballistic resistanceSpecification: 1200X1600mmApplication: 46 layers for 54 type lead core, 36 layers for NIJ Standard IIIAInformation provided by Beijing Evergrow Resources.
Descriptive Properties Value Comments
Area Density 157-163 cm²/g
Users viewing this material also viewed the following: