Beijing Evergrow Resources GFF-3 Glass Fiber Felt

Category Ceramic , Glass , Glass Fiber
Manufacturer Beijing Evergrow Resources
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Beijing Evergrow Resources GFF-3 Glass Fiber Felt.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Introduction:By applying high-count fiberglass, GFNF series has the excellent properties such as heat-isolation, fire-resistance, anti-corrosion and heat-preservation. It's the most characteristic and newest heat-preservation material of inorganic silicate at present.Features:Lightness, heat resisting, low thermal capacity and low thermal conductivity, soft and excellent fire-isolation.Anti-heat energy and heat stability.Anti-mildew, anti-insect, un-scattered and good stretching resistance.Excellent anti-ageing.Excellent sound absorbability, adsorption and filtering.It can be cut, sewn according to requirements and it's also easy to construct.Application:This mat is widely used for wrapping material of all kinds of heat source (coal, electricity, oil, and gas) and heat-presentation of central air-conditioning pipelines.It can be used as the materials for heat-isolation and fire-resistance.It can be used as the materials for seal, sound absorption filtering and insulation.Excellent material for heat-conducting, heat-presentation.It can be used as materials for sound isolation, heat insulation and heat-resistance in vehicles, vessels and aircrafts.It can also be used for touching fire and all kinds of flue in which the temperature is less than 600ºC.Information provided by Beijing Evergrow Resources.
Physical Properties Metric English Comments
Thickness >= 3000 microns
>= 118 mil
Mechanical Properties Metric English Comments
Tensile Strength at Break 4.00 MPa
580 psi
Thermal Properties Metric English Comments
Thermal Conductivity 0.0550 - 0.0640 W/m-K
0.382 - 0.444 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 600 °C
1110 °F
Descriptive Properties Value Comments
Weight (g/m²) 500-600
Width (mm) 1000-2000±50mm
Users viewing this material also viewed the following: