Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Borealis BorSafe™ HE3490-IM HDPE Compound for Injection Molded Pressure Fittings

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Borealis
Trade Name BorSafe™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis BorSafe™ HE3490-IM HDPE Compound for Injection Molded Pressure Fittings.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
BorSafe™ HE3490-IM is a bimodal polyethylene compound produced by the advanced Borstar® technology. Well dispersed carbon black gives outstanding UV resistance. Long term stability is ensured by an optimized stabilization system. BorSafe™ HE3490-IM is classified as an MRS 10.0 material (PE100). Applications: BorSafe™ HE3490-IM is especially designed for the injection molding of fittings in the application field of drinking water, natural gas, pressure sewerage, industrial, relining, and sea outfall.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.959 g/cc
0.0346 lb/in³
ISO 1872-2/ISO 1183
Environmental Stress Crack Resistance 1.0 hour

@Pressure 0.920 MPa,
Temperature 80.0 °C
1.0 hour

@Pressure 133 psi,
Temperature 176 °F
ISO 13479
Oxidative Induction Time (OIT) >= 20 min

@Temperature 200 °C
>= 20 min

@Temperature 392 °F
EN 728
Carbon Black Loading 2.0 %
2.0 %
ASTM D1603
Melt Flow 0.55 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.55 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.0 MPa
3480 psi
ISO 527-2
Elongation at Break >= 600 %
>= 600 %
ISO 527-2
Tensile Modulus 1.10 GPa
160 ksi
ISO 527-3
Processing Properties Metric English Comments
Melt Temperature 190 - 260 °C
374 - 500 °F
Descriptive Properties Value Comments
Carbon Black Dispersion < 3
ISO 18553
Users viewing this material also viewed the following: