Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Buckeye Polymers BP RPP 3005 GR BLK Polypropylene, Glass Filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 30% Glass Fiber Filler
Manufacturer Buckeye Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Buckeye Polymers BP RPP 3005 GR BLK Polypropylene, Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Information: Our glass reinforced product lines exhibit increased tensile strength, stiffness, and heat deflection. Highly optimized glass reinforced PP resins have successfully replaced engineering thermoplastics in numerous applications.Product Features:Chemically coupledGood flexural strengthInformation Provided by Buckeye Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.11 - 1.15 g/cc
1.11 - 1.15 g/cc
ASTM D792
Melt Flow 5.0 - 9.0 g/10 min
5.0 - 9.0 g/10 min
ASTM D1238
Ash 28 - 32 %
28 - 32 %
ASTM D5630
Mechanical Properties Metric English Comments
Flexural Modulus >= 4.139 GPa
>= 600.3 ksi
ASTM D790
Izod Impact, Notched >= 0.6401 J/cm
>= 1.199 ft-lb/in
ASTM D256
Users viewing this material also viewed the following: