Carmel Olefins CAPILENE® TG 50 Polypropylene Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Carmel Olefins
Trade Name CAPILENE®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Carmel Olefins CAPILENE® TG 50 Polypropylene Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: CAPILENE® TG 50 is a heterophasic copolymer designed for injection molding applications requiring optimal impact resistance. This grade combines excellent impact strength, even at low temperatures, with a fair stiffness level and moderate flow properties.Applications: CAPILENE® TG 50 is suitable for injection molding of household articles, crates, boxes, luggage, toys, technical items and paint pails.Information provided by Carmel Olefins.
Physical Properties Metric English Comments
Melt Flow 3.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.0 MPa
3190 psi
50 mm/min; ASTM D638
Elongation at Yield 10 %
10 %
50 mm/min; ASTM D638
Flexural Modulus 0.975 GPa
141 ksi
ASTM D790
Izod Impact, Notched 1.25 J/cm

@Temperature -20.0 °C
2.34 ft-lb/in

@Temperature -4.00 °F
ASTM D256
7.00 J/cm

@Temperature 23.0 °C
13.1 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C
176 °F
ASTM D648
Vicat Softening Point 145 °C

@Load 1.02 kg
293 °F

@Load 2.25 lb
ASTM D1525