Material Notes:
A non-halogenated, unfilled nylon 66 used in electrical applications where improved flame retardancy is required. The material has excellent moldability, good snap-fit properties and is available in a range of colors.Data provided by the manufacturer, Chem Polymer.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 72.0 MPa
10400 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Flexural Yield Strength 85.0 MPa
12300 psi
ASTM D790
Flexural Modulus 3.30 GPa
479 ksi
ASTM D790
Thermal Properties Metric English Comments
Melting Point 252 °C
486 °F
ASTM D789
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Comparative Tracking Index >= 600 V
>= 600 V
CTI, V
Processing Properties Metric English Comments
Melt Temperature 277 °C
531 °F