Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Cheng Yu Plastic PP231H TALC 40 Polypropylene, 40% Talc, High Heat

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Talc Filler
Manufacturer Cheng Yu Plastic Company Limited (formerly Luen Cheong Hong)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cheng Yu Plastic PP231H TALC 40 Polypropylene, 40% Talc, High Heat.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D792
Linear Mold Shrinkage 0.010 - 0.020 cm/cm
0.010 - 0.020 in/in
ASTM D955
Melt Index of Compound 20 g/10 min
20 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 100
100
ASTM D785
Tensile Strength, Yield 34.3 MPa
4980 psi
ASTM D638
Flexural Yield Strength 63.7 MPa
9250 psi
ASTM D790
Izod Impact, Notched 0.255 J/cm
0.478 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 140 °C
284 °F
ASTM D648
Flammability, UL94 HB
HB