| Category | Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled |
| Manufacturer | Cheng Yu Plastic Company Limited (formerly Luen Cheong Hong) |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Cheng Yu Plastic T890G3 PBT, 30% Glass Fiber.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.50 g/cc | 1.50 g/cc | ASTM D792 |
| Linear Mold Shrinkage | 0.0020 - 0.015 cm/cm | 0.0020 - 0.015 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 95 | 95 | ASTM D785 |
| Tensile Strength, Yield | 127 MPa | 18500 psi | ASTM D638 |
| Flexural Yield Strength | 191 MPa | 27700 psi | ASTM D790 |
| Izod Impact, Notched | 1.27 J/cm | 2.39 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 228 °C | 442 °F | ASTM D648 |
| Flammability, UL94 | HB | HB |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Constant | 3.7 @Frequency 60 Hz |
3.7 @Frequency 60 Hz |
ASTM D150 |