Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chevron Phillips 7109DLT LLDPE Blown Film Resin, Hexene Copolymer  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips 7109DLT LLDPE Blown Film Resin, Hexene Copolymer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Resin Type: Hexene Copolymer, Very High Antiblock, Processing Aid Version of 7109T, Cast/Blown Film ResinCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended with LDPE or HDPEApplications:Industrial Liners, Garment Bags, Carrier Bags, CoextrusionsProcessing Conditions: Extruder 6.35 cm. Screw L/D Ratio 24:1. Die Opening 0.1905 cm. Blow-Up Ratio 2:1.Film properties below based on film thickness of 31.8 µm. Antiblock 6500 ppm.Data provided by Chevron Chemical.
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ASTM D1505
Melt Flow 0.90 g/10 min
0.90 g/10 min
Condition E; ASTM D 1238
Mechanical Properties Metric English Comments
Coefficient of Friction 0.75
0.75
ASTM D1894
Dart Drop 4.20 g/micron
107 g/mil
F<sub>50</sub>; 1.5 in. dart/26 in. drop height; ASTM D 1709
Optical Properties Metric English Comments
Haze 12 %
12 %
ASTM D2457
Gloss 60 %
60 %
at 45°. ASTM D 2457
100 %
100 %
at 60°. ASTM D 2457
Processing Properties Metric English Comments
Melt Temperature 220 °C
428 °F
Copyright © lookpolymers.com All Rights Reserved