Material Notes:
Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 233, A 56700Characteristics: Moderate Flow, Excellent Impact Strength, Good Stiffness, Excellent ESCR, Moderate Shrinkage ResistanceApplications:Industrial Pails (5 gallon), Pail/Drum LidsData provided by Chevron Chemical.
Physical Properties Metric English Comments
Density 0.953 g/cc
0.0344 lb/in³
ASTM D1505
Apparent Bulk Density 0.590 g/cc
0.0213 lb/in³
ASTM D1895
Melt Flow 4.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
High Load Melt Index 117 g/10 min

@Load 21.6 kg,
Temperature 190 °C
117 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.9 MPa
3900 psi
ASTM D638
Elongation at Break 900 %
900 %
ASTM D638
Flexural Modulus 1.03 GPa
149 ksi
3 pt. secant; ASTM D790
1.28 GPa
186 ksi
3 pt. Tangent; ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 125 °C
257 °F
ASTM D1525
Brittleness Temperature <= -71.0 °C
<= -95.8 °F
ASTM D746