ChevronTexaco Gear Compounds EP J, ISO 220

Category Fluid , Lubricant
Manufacturer ChevronTexaco Corp
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco Gear Compounds EP J, ISO 220.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
FeaturesChevron Gear Compounds EP J are multipurpose gear lubricants.They are formulated with highly refined, high viscosity index paraffinic base oils and a new generation sulfurphosphorus additive system. Chevron Gear Compounds EP J contain extreme pressure, antiwear and emulsibility additives; oxidation, rust, corrosion and foam inhibitors; a pour point depressant; and a metal deactivator to protect copper or copper alloys from corrosion.They are specifically designed to meet or exceed the performance requirements of Joy Technologies specifications for transmission oils.Chevron Gear Compounds EP J are formulated to give high film strength and load-carrying capacity. Gear teeth are protected from wear, all types of surface distress, and premature failure.They provide improved thermal and oxidation stability to prevent degradation under severe operating conditions and provide longer lubricant life. They are designed to form a stable emulsion with contaminating water.ApplicationsChevron Gear Compounds EP J are recommended for use in Joy Technologies transmissions or other similar applications where water emulsifying gear oils are required.Chevron Gear Compounds EP J meet Joy specifications TO-MEP (ISO 220), TO HEP (ISO 320) and TO HD (ISO 460).For customers that do not have water emulsibility as a requirement, Chevron Gear Compounds EP or Chevron Ultra Gear Lubricants are recommended. Chevron Ultra Gear Lubricants can be used in industrial applications where overloading, severe operating conditions, high lubricant operating temperatures, or other problems are encountered.
Physical Properties Metric English Comments
API Gravity 28.1 °
28.1 °
Viscosity Measurement 104
104
Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 1158 SUS
1158 SUS
Saybolt Viscosity at 210°F 101 SUS
101 SUS
Kinematic Viscosity at 40°C (104°F) 220 cSt
220 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 19.9 cSt
19.9 cSt
ASTM D445
Mechanical Properties Metric English Comments
Falex Load Test >= 1.70e+6 g
>= 3750 lb
ASTM D3233
Thermal Properties Metric English Comments
Pour Point -24.0 °C
-11.2 °F
ASTM D97
Flash Point 248 °C
478 °F
ASTM D92
Descriptive Properties Value Comments
Corrosion, Copper Strip Test 3h 0 at 100°C
Emulsibility ASTM D1401, mL H20 at 48 h 0
Foaming Stability, mL 0
Foaming Tendency, mL 0
FZG Gear Wear Test, Failure Load Stage 12
Oxidation, ASTM D2893, % Viscosity Increase 3.2
Rust Prevention, ASTM D665 Pass