Category Fluid , Lubricant , Urea Gellant
Manufacturer ChevronTexaco Corp
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF ChevronTexaco Rykotac® Grease EP.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
FeaturesChevron Rykotac Grease EP is manufactured using highly refined, select high viscosity index base oils, and a polyurea thickener. It is red in color and tacky in texture.Chevron Rykotac Grease EP contains polyurea thickener, highly refined paraffinic base oil, extreme pressure agents, and a special combination of synthetic tackiness agents. These agents allow maximum tackiness with a wide temperature range for high and low temperature performance.ApplicationsChevron Rykotac Grease EP is an excellent choice for heavy duty construction equipment, fifth wheel, chain drives, and other applications in which a grease that clings to metal and resists spin-off is needed. These properties are given by a formulation balanced to provide good cold weather and high temperature performance.Chevron Rykotac Grease EP can be used in both plain and antifriction bearings.Applications include:Cement plantsConstructionFarmingMarineMiningOil fieldsPaper millsGeneral industryConveyor systems
Physical Properties Metric English Comments
Viscosity Measurement 171
171
Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 741 SUS
741 SUS
Saybolt Viscosity at 210°F 106 SUS
106 SUS
Kinematic Viscosity at 40°C (104°F) 145 cSt
145 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 21 cSt
21 cSt
ASTM D445
Mechanical Properties Metric English Comments
Penetration 260
260
Worked
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 177 °C
351 °F
Minimum Service Temperature, Air -34.0 °C
-29.2 °F
Dropping Point 260 °C
500 °F
Descriptive Properties Value Comments
Color Red
Texture Tacky
Thickener, % / type - / Polyurea
Water Resistance, 79°C, % loss 2