Material Notes:
High strength in use and good impact & shock resistance, yet lower than YT5,Rough turning and rough milling of carbon steel and alloy steel during continuous cutting or medium to fine turning of them during intermittent cuttingInformation provided by China Tungsten
Physical Properties Metric English Comments
Density 11.4 g/cc
0.412 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell A 91.5
91.5
Flexural Strength 1750 MPa
254000 psi