Physical Properties Metric English Comments
Bulk Density 3.05 - 3.15 g/cc
0.110 - 0.114 lb/in³
Porosity 4.0 - 8.0 %
4.0 - 8.0 %
Mechanical Properties Metric English Comments
Modulus of Rupture <= 0.012753 GPa

@Temperature 1400 °C
<= 1.8497 ksi

@Temperature 2550 °F
Compressive Strength <= 98.1 MPa
<= 14200 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
CTE, linear 9.00 - 11.0 µm/m-°C

@Temperature 1000 °C
5.00 - 6.11 µin/in-°F

@Temperature 1830 °F
Component Elements Properties Metric English Comments
Al2O3 88 - 93 %
88 - 93 %
Carbon, C 2.0 - 4.0 %
2.0 - 4.0 %
Descriptive Properties Value Comments
Remarks Excellent for high 0 steel, Excellent corrosion resistance