Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 2.90 g/cc
0.105 lb/in³
Porosity 15 %
15 %
Mechanical Properties Metric English Comments
Compressive Strength 83.4 MPa
12100 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
CTE, linear 6.80 µm/m-°C

@Temperature 1000 °C
3.78 µin/in-°F

@Temperature 1830 °F
Shrinkage -0.200 - 0.20 %

@Temperature 1600 °C,
Time 7200 sec
-0.200 - 0.20 %

@Temperature 2910 °F,
Time 2.00 hour
Component Elements Properties Metric English Comments
Al2O3 82 %
82 %
Fe2O3 0.80 %
0.80 %
Descriptive Properties Value Comments
Main Application Chemical Reactor, Incinerator, Various Non ferrous metal melting furnace
Refractories Under Load(2kg/?,T2?) 1,670
Refractoriness (SK) 39
Users viewing this material also viewed the following: