Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Colorite Polymers 8002 General Purpose Vinyl Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded
Manufacturer Colorite Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Colorite Polymers 8002 General Purpose Vinyl Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame retardance, low temperature, or chemical resistance, are all available. Formulations for exterior or interior use.Typical Applications: Clear General Purpose MoldingInformation provided by Colorite Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.23 g/cc
1.23 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
10 sec; ASTM D2240
Tensile Strength, Ultimate 18.6 MPa
2700 psi
ASTM D638
Elongation at Break 350 %
350 %
ASTM D638
100% Modulus 0.00862 GPa
1.25 ksi
ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature -28.0 °C
-18.4 °F
ASTM D746
Users viewing this material also viewed the following: