Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Colorite Polymers Self Frosting™ 6511SF Vinyl Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded
Manufacturer Colorite Polymers
Trade Name Self Frosting™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Colorite Polymers Self Frosting™ 6511SF Vinyl Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Colorite has developed a family of vinyl compounds to satisfy the needs of those who need a smooth, low gloss, low friction surface for the products that they produce. Historically, this was accomplished by using cold die techniques that reduced production rates by as much as 20%. This method also generates substantial amounts of scrap or rejected material due to imperfect frosting. Colorite SF compounds permit the user to maintain production rates with a uniform reproducible matte finish. Colorite SF compounds are available in non-toxic grades for the food and medical industries where the need for a low surface friction tubing exists and total transparency is not necessary.Information provided by Colorite Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 65
65
Tensile Strength, Ultimate 11.7 MPa
1700 psi
Elongation at Break 450 %
450 %
100% Modulus 0.00427 GPa
0.620 ksi
Thermal Properties Metric English Comments
Brittleness Temperature -44.0 °C
-47.2 °F
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved