| Category | Ceramic , Carbide |
| Manufacturer | CoorsTek |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | CoorsTek Tungsten Carbide, WC.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 14.9 g/cc | 0.538 lb/in³ | ASTM C20 |
| Water Absorption | 0.00 % | 0.00 % | ASTM C373 |
| Particle Size | 2.0 µm | 2.0 µm | Average Crystal Size - Thin Section Test |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Modulus of Elasticity | 627 GPa | 90900 ksi | ASTM C848 |
| Flexural Strength | 1930 MPa | 280000 psi | ASTM F417 |
| Compressive Strength | 5000 MPa | 725000 psi | ASTM C773 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 5.10 µm/m-°C @Temperature 25.0 - 1000 °C |
2.83 µin/in-°F @Temperature 77.0 - 1830 °F |
ASTM C372 |
| Thermal Conductivity | 100 W/m-K | 694 BTU-in/hr-ft²-°F | ASTM C408 |
| Maximum Service Temperature, Air | 1000 °C | 1830 °F | No Load |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Transmission, Visible | 0.00 % | 0.00 % |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | <= 1000 ohm-cm @Temperature 500 °C |
<= 1000 ohm-cm @Temperature 932 °F |
|
| <= 1000 ohm-cm @Temperature 1000 °C |
<= 1000 ohm-cm @Temperature 1830 °F |
||
| <= 1000 ohm-cm @Temperature 25.0 °C |
<= 1000 ohm-cm @Temperature 77.0 °F |