Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Cytec Thornel® T-650/42 12K Carbon Fiber, Polyacrylonitrile (PAN) Precursor

Category Carbon , Carbon Fiber , Other Engineering Material , Composite Fibers
Manufacturer Cytec
Trade Name Thornel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cytec Thornel® T-650/42 12K Carbon Fiber, Polyacrylonitrile (PAN) Precursor.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated to increase the interlaminar shear strength in a resin matrix composite.12000 filaments/strand, 94% carbon assay, 5.1 µm filament diameter, 2.27 m/g yield, 0 tpm twist (also available twisted), 0.246 mm² fiber area in yarn cross section.Thornel® products were sold by Amoco and are now owned by Cytec.
Physical Properties Metric English Comments
Density 1.78 g/cc
0.0643 lb/in³
Specific Surface Area 0.50 m²/g
0.50 m²/g
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 4820 MPa
699000 psi
Elongation at Break 1.7 %
1.7 %
Modulus of Elasticity 290 GPa
42100 ksi
In Tension
Thermal Properties Metric English Comments
CTE, linear -0.500 µm/m-°C

@Temperature 20.0 °C
-0.278 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 15.0 W/m-K
104 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 0.00142 ohm-cm
0.00142 ohm-cm