Denka VINYKON R3105 PVC, R grade for hard extrusion

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Denka
Trade Name VINYKON
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Denka VINYKON R3105 PVC, R grade for hard extrusion.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding, etc.
Physical Properties Metric English Comments
Density 1.401 g/cc
0.05061 lb/in³
JIS-Z-8807
Mechanical Properties Metric English Comments
Tensile Strength at Break 46.01 MPa
6673 psi
JIS-K-6740
Elongation at Break 127 %
127 %
JIS-K-6740
Flexural Strength 65.0 MPa
9430 psi
JIS-K-6740
Flexural Modulus 2.49 GPa
361 ksi
JIS-K-6740
Izod Impact, Notched 0.44145 J/cm

@Temperature -20.0 °C
0.82702 ft-lb/in

@Temperature -4.00 °F
JIS-K-6740
0.81423 J/cm

@Temperature 0.000 °C
1.5254 ft-lb/in

@Temperature 32.0 °F
JIS-K-6740
2.6487 J/cm

@Temperature 23.0 °C
4.9621 ft-lb/in

@Temperature 73.4 °F
JIS-K-6740
Penetration 74
74
[°C], penetration temperature; JIS-K-6740
Thermal Properties Metric English Comments
Vicat Softening Point 86.0 °C
187 °F
JIS-K-6740
Descriptive Properties Value Comments
Thermostability, min, JIS-K-6723 70