Material Notes:
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding, etc.
Physical Properties Metric English Comments
Density 1.382 g/cc
0.04993 lb/in³
JIS-Z-8807
Deformation 3.0 %
3.0 %
JIS-K-6723
Mechanical Properties Metric English Comments
Hardness, Shore A 98
98
JIS-K-6301
Tensile Strength at Break 32.373 MPa
4695.3 psi
JIS-K-6723
Elongation at Break 280 %
280 %
JIS-K-6723
100% Modulus 0.024525 GPa
3.5571 ksi
JIS-A-5756
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -12.0 °C
10.4 °F
JIS-K-6723
Electrical Properties Metric English Comments
Volume Resistivity 5.00e+13 ohm-cm

@Temperature 60.0 °C
5.00e+13 ohm-cm

@Temperature 140 °F
JIS-K-6723
5.00e+14 ohm-cm

@Temperature 30.0 °C
5.00e+14 ohm-cm

@Temperature 86.0 °F
JIS-K-6723
Descriptive Properties Value Comments
Heating: Retention Rate of Elongation, % 97
JIS-A-5756
Heating: Retention Rate of Tensile Strength, % 97
JIS-A-5756
Oil Resistance: Retention of Tensile Strength, % 90
JIS-K-6723
Oil Resistance: Retention Rate of Elongation, % 87
JIS-K-6723
Thermostability, min, JIS-K-6723 >240