Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow Saran® 8 Clear Plastic Barrier Film

Category Polymer , Film , Thermoplastic , PVDC
Manufacturer Dow Chemical
Trade Name Saran®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Saran® 8 Clear Plastic Barrier Film.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Saran™ 8 is a clear biaxially oriented monolayer barrier film, designed for tight wrap and heat sealing applications. It is available in 50 gauge, as single or double wound rolls.Information provided by Dow
Physical Properties Metric English Comments
Water Vapor Transmission 9.00 g/m²/day
0.580 g/100 in²/day
at 100°F, 90% RH; ASTM F1249-90
Oxygen Transmission 0.512 cc-mm/m²-24hr-atm
1.30 cc-mil/100 in²-24hr-atm
10% RH; ASTM D3985
Thickness 15.2 microns
0.600 mil
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 75 %
75 %
ASTM D882
Film Elongation at Break, TD 55 %
55 %
ASTM D882
Secant Modulus, MD 0.6895 GPa
100.0 ksi
2% Secant; ASTM D882
Secant Modulus, TD 0.6205 GPa
90.00 ksi
2% Secant; ASTM D882
Film Tensile Strength at Break, MD 75.8 MPa
11000 psi
ASTM D882
Film Tensile Strength at Break, TD 124 MPa
18000 psi
ASTM D882
Thermal Properties Metric English Comments
Shrinkage, MD 16 %
16 %
Unrestrained, 100°C Air; ASTM D1204
Shrinkage, TD 9.0 %
9.0 %
Unrestrained, 100°C Air; ASTM D1204
Optical Properties Metric English Comments
Haze 1.0 %
1.0 %
ASTM D1003
Gloss 115 %
115 %
45°; ASTM D2457
Transmission, Visible 73 %
73 %
Clarity; ASTM D1746
Descriptive Properties Value Comments
Block Force g 114
ASTM D3354-89, unconditioned
Cling g 65
ASTM D4649-87, unstretched
Yield in2/lb 27000
Calculated