DuPont Teijin Films Melinex® 342 Polyester Film

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Melinex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Melinex® 342 Polyester Film.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Melinex® 342 is a two-side heat-sealable, clear polyester film which is ideal in specialty card laminate applications. This film can be heat sealed to itself and other polyesters, as well as a variety of substrates including some grades of paper, PVC, and Teslin®. Melinex® 342 film is currently available in thicknesses of 400 and 600 gauge.Information provided by DuPont.
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
ASTM D1505
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 180 %
180 %
ASTM D882A
Film Elongation at Break, TD 130 %
130 %
ASTM D882A
Coefficient of Friction, Dynamic 0.90
0.90
A-B; ASTM D1894
Film Tensile Strength at Break, MD 165 MPa
24000 psi
ASTM D882A
Film Tensile Strength at Break, TD 165 MPa
24000 psi
ASTM D882A
Heat Seal Strength 1500 g/25 mm

@Time 2.00 sec,
Pressure 0.276 MPa
3.31 lb/in

@Time 0.000556 hour,
Pressure 40.0 psi
DuPont 275°F, (HS/HS)
Heat Seal Strength Initiation Temperature 135 - 191 °C
275 - 375 °F
1 sec @40 psi
Thermal Properties Metric English Comments
Shrinkage, MD 2.0 %

@Temperature 190 °C,
Time 300 sec
2.0 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 2.0 %

@Temperature 190 °C,
Time 300 sec
2.0 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Optical Properties Metric English Comments
Transmission, Visible 86 %

@Thickness 0.152 mm
86 %

@Thickness 0.00600 in
TLT; ASTM D1003
87 %

@Thickness 0.102 mm
87 %

@Thickness 0.00400 in
TLT; ASTM D1003