Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Teijin Films Melinex® 606 Polyester Film, 300 Gauge

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Melinex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Melinex® 606 Polyester Film, 300 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Melinex® 606 is a very smooth two-side coated polyester film designed specifically for high density floppy disks.Also available in 285 GaugeInformation provided by DuPont.
Physical Properties Metric English Comments
Density 1.395 g/cc
0.05040 lb/in³
ASTM D1505
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 95.8 MPa

@Strain >=5.00 %
13900 psi

@Strain >=5.00 %
ASTM D882A
Film Tensile Strength at Yield, TD 95.8 MPa

@Strain >=5.00 %
13900 psi

@Strain >=5.00 %
ASTM D882A
Secant Modulus, MD 3.39 GPa
492 ksi
ASTM D882A
Secant Modulus, TD 4.21 GPa
610 ksi
ASTM D882A
Film Tensile Strength at Break, MD 191 MPa
27700 psi
ASTM D882A
Film Tensile Strength at Break, TD 225 MPa
32600 psi
ASTM D882A
Thermal Properties Metric English Comments
Shrinkage, MD 2.5 %

@Temperature 190 °C,
Time 300 sec
2.5 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 1.0 %

@Temperature 190 °C,
Time 300 sec
1.0 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Optical Properties Metric English Comments
Transmission, Visible 90.2 %
90.2 %
TLT; ASTM D1003
Descriptive Properties Value Comments
Coefficient of Hygroscopic Expansion 7E-06
per 40% - 80% RH