Material Notes:
High Specific Gravity, Tungsten Powder Filled Co-Polyamide (COPA), Excellent Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing and radiation shielding applicationsInformation provided by Technical Polymers.
Physical Properties Metric English Comments
Specific Gravity 10.0 g/cc
10.0 g/cc
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 26.5 MPa
3850 psi
ASTM D638
Elongation at Break 4.5 %
4.5 %
ASTM D638
Tensile Modulus 4.83 GPa
700 ksi
ASTM D638
Flexural Strength 79.3 MPa
11500 psi
ASTM D790
Flexural Modulus 3.59 GPa
520 ksi
ASTM D790
Izod Impact, Notched 1.33 J/cm
2.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 65.6 °C
150 °F
ASTM D648
Electrical Properties Metric English Comments
Surface Resistivity per Square 0.20 ohm
0.20 ohm
ASTM D257
Processing Properties Metric English Comments
Melt Temperature 232 - 249 °C
450 - 480 °F
Mold Temperature 65.6 - 82.2 °C
150 - 180 °F
Drying Temperature 73.9 °C
165 °F
Dry Time 4 hour
4 hour