Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ensinger Tecapeek® XP-113 Compression Molded PEEK Compound, 10% PTFE, 15% Graphite, and 3% Carbon Fiber

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Carbon Fiber Filled , Polyetheretherketone, PEEK, PTFE-Filled
Manufacturer Ensinger
Trade Name Tecapeek®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger Tecapeek® XP-113 Compression Molded PEEK Compound, 10% PTFE, 15% Graphite, and 3% Carbon Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in lower amounts of scrap, uniform physical properties and fewer molded-in stresses.TECAPEEK is a high-perfomance engineering thermoplastic. This semi-crystalline material has a balance of high temperature mechanical properties, chemical and steam resistance, superior wear properties and processability which makes it unique.Applications Include:Bearings and BushingsDown-hole instrumentationWear RingsBall Valve SeatsElectrical ComponentsBack-up and V-RingsPiston Rings and Rider BandsInformation provided by Ensinger Special Polymers, Inc.
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0531 lb/in³
ASTM D792
Filler Content 25 %
25 %
Mechanical Properties Metric English Comments
Hardness, Rockwell M 96
96
ASTM D785
Tensile Strength 51.7 MPa
7500 psi
ASTM D638
Elongation at Break 1.3 %
1.3 %
ASTM D638
Tensile Modulus 4.83 GPa
700 ksi
ASTM D638
Flexural Strength 82.7 MPa
12000 psi
ASTM D790
Flexural Modulus 4.83 GPa
700 ksi
ASTM D790
Compressive Strength 117 MPa
17000 psi
ASTM D695
Thermal Properties Metric English Comments
Melting Point 343 °C
649 °F
DSC
Descriptive Properties Value Comments
Color Black
Users viewing this material also viewed the following: