Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil EXACT™ 4150 Plastomer

Category Polymer , Film , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO), Film Grade , Polyethylene (PE)
Manufacturer Exxon Chemical
Trade Name EXACT™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil EXACT™ 4150 Plastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: Exact 4150 is an ethylene-based hexane plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 4150 is designed for multilayer coextruded cast film applications requiring low sealing temperatures, high oxygen transmission, and high toughness. Typical applications include seal layers for lamination films used in meat, poultry, and fresh produce packaging.Availability: Latin America, North America and South America Additive: Antiblock: NoSlip: No Thermal Stabilizer: YesApplications:Cast FilmLamination Film Data provided by the manufacturer, Exxon Chemical.
Physical Properties Metric English Comments
Density 0.895 g/cc
0.0323 lb/in³
Exxon Method
Thickness 20.3 microns
0.800 mil
Melt Flow 3.5 g/10 min
3.5 g/10 min
Exxon Method
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 4.76 MPa
690 psi
ASTM D882
Film Tensile Strength at Yield, TD 4.21 MPa
611 psi
ASTM D882
Film Elongation at Break, MD 470 %
470 %
ASTM D882
Film Elongation at Break, TD 660 %
660 %
ASTM D882
Film Elongation at Yield, MD 10 %
10 %
ASTM D882
Film Elongation at Yield, TD 9.0 %
9.0 %
ASTM D882
Secant Modulus, MD 0.0552 GPa
8.01 ksi
ASTM D882
Secant Modulus, TD 0.0593 GPa
8.60 ksi
ASTM D882
Puncture Energy 5.31 J
3.92 ft-lb
ExxonMobil Method
Elmendorf Tear Strength, MD 7.87 g/micron
200 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 17.2 g/micron
438 g/mil
ASTM D1922
Dart Drop 26.6 g/micron
675 g/mil
ASTM D1709
Film Tensile Strength at Break, MD 75.8 MPa
11000 psi
ASTM D882
Film Tensile Strength at Break, TD 68.9 MPa
9990 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point 89.0 °C
192 °F
Exxon Method
Crystallization Temperature 162 °C
324 °F
ExxonMobil Method
Vicat Softening Point 167 °C
333 °F
ASTM D1525
Optical Properties Metric English Comments
Haze 0.10 %
0.10 %
ASTM D1003
Gloss 97 %
97 %
45°; ASTM D2457
Descriptive Properties Value Comments
Puncture Force 12 lbf
ExxonMobil Method
Users viewing this material also viewed the following: