Material Notes:
Exxpro Elastomer is a brominated copolymer of isobutylene and paramethylstyrene. The product form is off whtie to amber bales.Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
Mooney Viscosity 40 - 50

@Temperature 125 °C
40 - 50

@Temperature 257 °F
ML 1 + 8; ASTM D1646
45

@Temperature 125 °C
45

@Temperature 257 °F
ML 1 + 8, Target; ASTM D1646
Maximum Moisture Content 0.30
0.30
Component Elements Properties Metric English Comments
Calcium, Ca 0.090 %
0.090 %
Target
0.070 - 0.11 %
0.070 - 0.11 %
Descriptive Properties Value Comments
Bromine 0.42-0.52%
mol %
0.47%
mol %, Target