Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil EXXPRO™ 3745 High Cure Activity Grade

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Exxon Chemical
Trade Name EXXPRO™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil EXXPRO™ 3745 High Cure Activity Grade.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Exxpro Elastomer is a brominated copolymer of isobutylene and paramethylstyrene. The product form is off whtie to amber bales.Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
Mooney Viscosity 40 - 50

@Temperature 125 °C
40 - 50

@Temperature 257 °F
ML 1 + 8; ASTM D1646
45

@Temperature 125 °C
45

@Temperature 257 °F
ML 1 + 8, Target; ASTM D1646
Maximum Moisture Content 0.30
0.30
Component Elements Properties Metric English Comments
Calcium, Ca 0.090 %
0.090 %
Target
0.070 - 0.11 %
0.070 - 0.11 %
Descriptive Properties Value Comments
Bromine, Benzylic 1.1-1.3%
mol %
1.2 %
mol %, Target
Users viewing this material also viewed the following: