Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil HDPE HD 7800P High Density Polyethylene Copolymer Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Exxon Chemical
Trade Name HDPE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil HDPE HD 7800P High Density Polyethylene Copolymer Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: HD 7800P is a pipe extrusion grade high density polyethylene copolymer offering an excellent combination of stiffness and stress crack resistance. This material meets or exceeds the AASHTO M294.Availability: Latin America, North America and South America Additive: Thermal Stabilizer: YesAntistatic: NoApplications: Agriculture Products ContainersCaps and ClosuresFood packagingHighway Drainage PipHousehold and Industrial chemical containersThermoformed PartsThin Gauge SheetInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.953 g/cc
0.0344 lb/in³
ExxonMobil method
Melt Flow 0.25 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.25 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
30 g/10 min

@Load 21.6 kg,
Temperature 190 °C
30 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.3 MPa
4100 psi
ASTM D638
Flexural Modulus, 1% Secant 965 MPa
140000 psi
ASTM D790
Descriptive Properties Value Comments
Notched Constant Ligament Stress (NCLS) ASTM F2136
Users viewing this material also viewed the following: