ExxonMobil Label-Lyte® 70 LS-447 Matte Finish, Coated, White Opaque, Sheetable OPP

Category Polymer , Adhesive , Film , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Exxon Chemical
Trade Name Label-Lyte®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Label-Lyte® 70 LS-447 Matte Finish, Coated, White Opaque, Sheetable OPP.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Coated, white, polypropylene film designed for use in hot melt cut-and-stack labeling. It has an anti-static, matte finish, paper-like print surface that is litho-printable, as well as compatible with solvent-based or water-based flexo and gravure inks and UV-cured inks. This film is designed to be used as a monoweb and provides excellent converting performance, including printing, sheeting, guillotine cutting, and label transfer on magazine-fed labelers. Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Thickness 76.2 microns
3.00 mil
Coating Weight >= 51.5 g/m²
>= 32.2 lb/ream
520
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 165 %
165 %
510
Film Elongation at Break, TD 40 %
40 %
510
Film Tensile Strength at Break, MD 73.546 MPa
10667 psi
510
Film Tensile Strength at Break, TD 149.39 MPa
21667 psi
510
Thermal Properties Metric English Comments
Shrinkage, MD 4.0 %
4.0 %
at 275°F; 438
Shrinkage, TD 4.5 %
4.5 %
at 275°F; 438
Optical Properties Metric English Comments
Gloss 10 %
10 %
442
Transmission, Visible 15 %
15 %
417
Descriptive Properties Value Comments
Gurley Stiffness, MD, mgf 29
Gurley Stiffness, TD, mgf 50
Yield, in2/lb 13400