ExxonMobil Santoprene® 283-40MED Thermoplastic Elastomer  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Santoprene® 283-40MED Thermoplastic Elastomer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of our medical grades. Prior to release, each medical grade lot undergoes a Cytotoxicity study using the ISO elution method and a Physico-Chemical - Elastomeric Closures test for heavy metals such as lead. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding, extrusion or blow molding. It is polyolefin based and completely recyclable.Information provided by Advanced Elastomer Systems
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
23°C; ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 39
39
.12 in; ASTM D2240
Tensile Strength at Break 14.28 MPa
2071 psi
Air at 212°F, 168 hr; ASTM D573
15.0 MPa
2180 psi
Across Flow; ASTM D412
Tensile Strength, Ultimate 8.48 MPa
1230 psi
Across Flow; ASTM D412
Elongation at Break 480.6 %
480.6 %
Air at 212°F, 168 hr; ASTM D573
540 %
540 %
Across Flow; ASTM D412
Tear Strength 28.0 kN/m
160 pli
212°F, Die C; ASTM D624
54.0 kN/m
308 pli
73°F, Die C; ASTM D624
Compression Set 43 %
43 %
73°F, 168 hr; ASTM D395
60 %
60 %
212°F, 168 hr; ASTM D395
Processing Properties Metric English Comments
Processing Temperature 175 - 230 °C
347 - 446 °F
Descriptive Properties Value Comments
Color Natural Color
Form Pellets