Material Notes:
Product Description: SpectraSyn™ Low Viscosity Polyalphaolefin (PAO) basestocks feature low temperature properties, low volatility, and improved thermal stability. SpectraSyn™ Low Viscosity (PAO) products have high viscosity indices which translate to improved flow at low temperatures and increased film thickness at high temperatures. SpectraSyn™ Low Viscosity PAO products are the primary basestocks for synthetic lubricants used in passenger car engines, heavy-duty diesel engines, transmissions, gear boxes and a variety of industrial applications. Appearance: Bright & ClearAvailability: Africa & Middle East, Asia Pacific, Central America, Europe, North America and South AmericaInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.820 g/cc
<br>@Temperature 15.6 °C
0.0296 lb/in³
<br>@Temperature 60.1 °F
ASTM D4052
Viscosity <= 1.46 cP
<= 1.46 cP
High-Temp. High Shear; ASTM D5481
<= 5000 cP
<br>@Temperature -40.0 °C
<= 5000 cP
<br>@Temperature -40.0 °F
Apparent Viscosity by Mini-Rotary Viscometer; ASTM D4684
Brookfield Viscosity 2500 cP
<br>@Temperature -40.0 °C
2500 cP
<br>@Temperature -40.0 °F
ASTM D2983
Viscosity Measurement 126
126
Index; ASTM D2270
Kinematic Viscosity 14500 cSt
<br>@Temperature -47.8 °C
14500 cSt
<br>@Temperature -54.0 °F
ASTM D445
29000 cSt
<br>@Temperature -40.0 °C
29000 cSt
<br>@Temperature -40.0 °F
ASTM D445
Kinematic Viscosity at 40°C (104°F) 19 cSt
19 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 4.1 cSt
4.1 cSt
ASTM D445
Vapor Pressure 0.000267 bar
<br>@Temperature 150 °C
0.200 torr
<br>@Temperature 302 °F
ASTM D2879
Evaporation Loss 1.6 %
<br>@Temperature 150 °C,<br> Time 79200 sec
1.6 %
<br>@Temperature 302 °F,<br> Time 22.0 hour
ASTM D972
Thermal Properties Metric English Comments
Pour Point -66.1 °C
-87.0 °F
ASTM D5950/D97
Flash Point 220 °C
428 °F
COC; ASTM D92
Optical Properties Metric English Comments
Refractive Index 1.4535
1.4535
ASTM D1218
Electrical Properties Metric English Comments
Dielectric Constant 2.1
2.1
ASTM D924
Dielectric Breakdown 43600 V
43600 V
Chemical Properties Metric English Comments
Acid Value <= 0.050
<= 0.050
[mg KOH/g]; ASTM D974 (mod)
Descriptive Properties Value Comments
Aniline Point 246.6°F
ASTM D611
Cold Cranking Simulator 1424 cP
-31°F, ASTM D5293
910 cP
-22°F, ASTM D5293
Color <0.5
ASTM D1500
Composition Water
&lt;50 ppm, ASTM D6304 (mod)
Density Correction Factor 0.000641 (g/cc)/°C
ASTM D1250
Fire point 493°F
COC, ASTM D92
Noack Volatility <14%
ASTM D5800/DIN 51581