Formosa Plastics Formolon® 165 PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Formosa Plastics Corporation, USA
Trade Name Formolon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolon® 165 PVC.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
PVC Copolymer Suspension Resin F-165 has been developed primarily to meet the processing requirements of the vinyl composition tile (VCT) manufacturers. In addition to vinyl floor tile industry, F-165 has found success in protective and strippable coatings.Information provided by Formosa Plastics Corporation, USA
Physical Properties Metric English Comments
Bulk Density 0.630 g/cc
0.0228 lb/in³
ASTM D1895
Volatiles 0.70 %
0.70 %
ASTM D3030
Particle Mesh Size 40 Mesh
40 Mesh
99.9% thru; ASTM D1921B
Viscosity 0.55 cP
0.55 cP
Inherent; ASTM D1243
Relative Viscosity 1.65 cP
1.65 cP
QC-10-104
Vinyl Acetate Content 13 %
13 %
QC-10-105
Descriptive Properties Value Comments
K-Value 52
Fikentscher's Constant