Freudenberg Simrit Hydrolysis-Resistant Polyurethane Elastomer

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer Freudenberg Simrit
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Freudenberg Simrit Hydrolysis-Resistant Polyurethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Developed for the Drinking Water Sector. Free of plasticisers. With hydrolysisresistant polyurethanes which have been specially developed with drinking water applications in mind, Simrit is now offering an interesting alternative to conventional materials which features many benefits, including Excellent wear resistance, Highly adjustable hardness range; Good tensile strength and breaking elongation; Resistance to mineral oils in wide temperature ranges; High ozone and oxidation resistance; Excellent damping behaviour; Enormous resistance to crack formation and crack growth.Information provided by Freudenburg-NOK.
Mechanical Properties Metric English Comments
Hardness, Shore A 85 - 94
85 - 94